Characteristics
| Feature | Description |
| Strength | Has higher strength compared to 3003 alloy. |
| Workability | Exhibits excellent workability in the annealed state. |
| Heat Treatment | Cannot be strengthened through heat treatment. |
| Anodizing | Suffers from severe anodizing color differences, thus is generally not suitable for anodizing processing. |
Due to the presence of magnesium in 3004 alloy, the main processing method is hot - rolling. This technique helps in achieving the desired properties and form of the alloy for different applications.
| Element | Composition Range (%) |
| Aluminum (Al) | Balance (≈97.5–98.5%) |
| Manganese (Mn) | 1.0–1.5% |
| Silicon (Si) | ≤0.35% |
| Iron (Fe) | ≤0.7% |
| Magnesium (Mg) | ≤0.25% |
| Copper (Cu) | ≤0.20% |
| Zinc (Zn) | ≤0.25% |
| Other Elements |
≤0.15% (each ≤0.05%)
|